You can see where around corners and even some straight runs it is peeling up. I’m running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I’ve trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

You are viewing a single thread.
View all comments View context

Seconded (or thirded?) I have a (textured) glass bed and my first layer is usually quite a bit more squished than this